MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PE-LD Soft PE, high-pressure PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: LD-PE is soft and particularly flexible. It is resistant to low temperatures of up to –50 °C and high temperatures of max. +60 °C.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³DIN EN ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454DIN EN ISO 868
Ball Indentation Hardness 21.0 MPa3050 psiDIN EN ISO 2039-1
Tensile Strength, Yield 13.0 MPa1890 psi50 mm/min; DIN EN ISO 527
Elongation at Yield 12 %12 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 0.350 GPa50.8 ksi1 mm/min; DIN EN ISO 527
Charpy Impact Unnotched NBNBDIN EN ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Strength 45.0 kV/mm1140 kV/inIEC 60243
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C111 µin/in-°FDIN 53752
Thermal Conductivity 0.320 W/m-K2.22 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 80.0 °C176 °Flong term
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
Colornatural(opal)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP002 / 250500

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.