Perkadox L-50S-PS is a 50% formulation in paste form. CAS number: 94-36-0 EINECS/ELINCS No.: 202-327-6 Applications: Perkadox L-50S-PS is a monofunctional peroxide which is used for the crosslinking of silicone rubber. Safe processing temperature: 85°C (rheometer ts2 > 20 min.). Typical crosslinking temperature: 105°C (rheometer t90 about 12 min.). Information provided by Nouryon |