Product description: Sipchem PBT-R1-B0-100 is a Polybutylene Terephthalate resin, manufactured by Sipchem Chemical Company in The Kingdom of Saudi Arabia using an Inventa-Fischer Technology. PBT-R1-B0-100 is a very low viscosity neat PBT resin Applications: Compounding Information provided by Sahara International Petrochemical Company |