MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Oschatz-Glas PD PowerStrand® HMW223-430L5 Textile Glass
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: The solution for applications where conventional E-glass fibers have reached their limits! A high modulus glass scores with strong performance for extreme demands. Whether used as roving, cut glass or fabric in combination with other materials, with ® Oschatz-Glas has created a reliable product that guarantees protection and safety in both the private and public sector. PD PowerStrand® is characterized by far better physical properties compare to E-glass fibers. Particularly higher tensile strength and increased impact resistance are the most important properties for this glass fiber type. Key facts for many applications are positive properties such a slow dead weight, fire and smoke protection, sound insulation as well as radio and radar permeability.

ADVANTAGE:

  • Better mechanical values (Strength und E-Modulus)
  • higher tensile strength
  • increased impact resistance
  • fire protection
  • noise protection
  • non conducting
  • low weight
  • radio waves and radar permeability remain
  • insulations
APPLICATIONS:
  • roving / automotive: timing belt
  • roving fabric / aircraft: Laminate in the aircraft; Floor plates; Interior
  • roving fabric / ballistics: panels for body armors; helmets; vehicle armor; object protection; shatter protection; Chopped strands / domestic appliance

Information provided by Oschatz-Glas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition 0.25 - 0.65 %DIN ISO 1887
Thickness 500 micronsISO 4603
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.15 %DIN EN ISO 3344
 
Descriptive Properties
Material2040 texwarp, DIN EN 12654
 2040 texweft, DIN EN 12654
Number of Threads19 1/cmwarp, ISO 1049
 19 1/cmweft, ISO 1049
Weave PaternplainISO 9354
Weight per unit area430 g/m²DIN EN 12127

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EOSCH967 / 320948

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.