MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot BLACK PEARLS® 4350 Specialty carbon black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: BLACK PEARLS 4350 specialty carbon black is a High Purity Furnace Black that meets the following purity requirements as required by the U.S. Food & Drug Administration (FDA): Total polyaromatic hydrocarbons (PAHs) not to exceed 0.5 parts per million (ppm) and Benzo[a]pyrene not to exceed 5.0 parts per billion (ppb). As a result of a new Food Contact Notification (FCN) submitted by Cabot to FDA (FCN 1789), BLACK PEARLS 4350 can be used in various food contact applications, including: as a component of adhesives; as a colorant in resinous and polymeric coatings; as a colorant in paper and paperboard in contact with aqueous and fatty foods; as a colorant in paper and paperboard in contact with dry foods; and as a colorant for polymers. It is to be used at levels not to exceed the minimum required to accomplish the intended technical effect. It is not for use in contact with infant formula and human milk.

Key applications: BLACK PEARLS 4350 specialty carbon black can be used in various food contact applications where FDA requirements are needed. This product also complies with regional food contact legislation such as European Union (Reg. No. 10/2011), Japan, China, and other regions. Example applications include:

  • Rigid food packaging
  • Flexible food packaging
  • Thermoformed trays
  • Non-food applications where high purity is desired such as parts that carry the GS (Geprüfte Sicherheit) Mark Certification and Regulation (EU) No 1272/2013, amending Annex XVII of REACH Regulation
Cabot Corporation uses a robust testing protocol to certify that BLACK PEARLS 4350 specialty carbon black meets the required purity levels and can be used in FDA plastics applications.

Performance features: BLACK PEARLS 4350 specialty carbon black exhibits a similar level of jetness and blue undertone as Cabot’s ELFTEX® 570 specialty carbon black, enabling good color and covering power. In addition, it has excellent dispersability and masterbatch dilutability.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Iodine absorption116 mg/gASTM D-1510
OAN70 cc/100gASTM D-2414
Product FormPellets
Tint1.18ASTM D-3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT030 / 315765

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.