LNP LUBRICOMP IFL36L compound is based on Nylon 6/12 resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Low Extractable, Wear Resistant. Features: Low Extractable,Wear resistant,Food Contact Acceptable,Structural Information provided by SABIC |