MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEMFR-ZHS Zinc Hydroxystannate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 12027-96-2

Advantages:

  • GOYENCHEMFR-ZHS is non-toxic and low heat release flame retardant which contains the fire resistant and inhibits fuming effects.
  • GOYENCHEMFR-ZHS mainly as a flame retardant and smoke inhibitor in the plastic industry.
  • GOYENCHEMFR-ZHS can replace antimony trioxide with better fire resistance.
  • GOYENCHEMFR-ZHS an environmentally product which is non-toxic and easy to use……etc.
Applications:
  • It can widely apply to plastic and high-end plastic products.
  • Conducting wire , wire and cable insulation
  • Construction material and painting

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size <= 2.0 µm
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl <= 0.10 %
Lead, Pb <= 0.0010 %
Tin, Sn 40 - 43 %
Zinc, Zn 21 - 24 %
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN154 / 266462

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.