MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alfa Chemistry Materials Cobalt Nanoparticle Dispersion
Categories: Metal; Nonferrous Metal; Cobalt Alloy

Material Notes: Synonyms: aqueous cobalt nanoparticle solution, cobalt nanofluid

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.100 - 0.250 g/cc0.00361 - 0.00903 lb/in³
Density 8.90 g/cc0.322 lb/in³
Specific Surface Area 40 - 60 m²/g40 - 60 m²/g
Molecular Weight 58.93 g/mol58.93 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 10431043MPa Microhardness
Modulus of Elasticity 209 GPa30300 ksi
Poissons Ratio 0.310.31
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.0 µm/m-°C
@Temperature 25.0 °C
7.22 µin/in-°F
@Temperature 77.0 °F
 
Descriptive Properties
Alfa Chemistry Materials CategoryMetals and Materials
AppearanceLiquid dispersion
CAS Number7440-48-4
EC Number231-158-0
GHS Hazard statementsH317-H334-H413
GHS Safety Description22-24-37-61
Hazard CodesXn
MDL NumberMFCD00010935
Molecular FormulaCo
MorphologySphere
particle size28 nm
Purity99%, 99.9%, 99.99%, 99.999%
Risk Codes42/43-53
Signal WordDanger
Size Range2-60 nm
UN NumberUN 3089 4.1/PG 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA0861 / 269801

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.