MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chemours Zonyl™ MPD 1700 PTFE Additive Dispersion
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Zonyl™ MPD 1700 is a milky-white, aqueous, PTFE dispersion stabilized with a non-ionic surfactant. Unlike most other grades of PTFE dispersions, Zonyl™ MPD 1700 is based on low molecular weight PTFE. It is designed to be used as an additive in host systems, in order to impart some of the unique properties of PTFE. The low molecular weight may make it unsuitable in some applications that require the physical properties of the high molecular weight grades. When properly processed, the PTFE resin in Zonyl™ MPD 1700 exhibits the superior properties typical of the fluoroplastic resins. Features: Inertness to nearly all industrial chemicals and solvents, Stability at high temperatures, Excellent dielectric properties, Lowest coefficient of friction of any solid material, Excellent weatherability, Non-stick characteristics. Applications: Additive for paints and coatings, Provides anti-stick surfaces, Reduces surface abrasion, Reduces internal friction, such that application is easier, Provides moisture protection, De-molding, Lubrication. Properly processed products (sintered at high temperatures common to the industry) made from Zonyl™ MPD 1700 resin can qualify for use in contact with food in compliance with FDA 21 CFR 177.1550 and European Regulation (EU) No. 10/2011.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccat 60% solids; ASTM D4441-04
Solids Content 60 %% PTFE by weight; ASTM D4441-04
pH 10.5Dispersion; ASTM E70
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Surfactant Content on PTFE Solids (%)6ASTM D4441-04

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8858 / 268785

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.