Appearance: Black Mix Ratio, by weight -Material:Catalyst: 100:4 Mix Ratio, by Volume -Material:Catalyst: 100:9.9 Product Benefits: - Thermally conductive
- Non-sag
- Thixotropic
- Resin versatility
- Low CTE
- Long pot life
- Good chemical resistance
- Good physical and chemical properties at elevated temperatures
Cure: Heat cureApplication: Thermally conductive adhesive Typical Assembly Applications: Bonding metals and ceramic substrates in heat sink applications LOCTITE ABLESTIK 285 CAT 11 adhesive is designed for assembly applications that require thermal management. It is also recommended for low stress bonding applications. LOCTITE ABLESTIK 285 CAT 11 can be used with a variety of catalysts. Information provided by Loctite® |