Veradel® 3300 Prem MR is a medium melt flow general purpose amorphous PESU resin with mold release for injection molding. This transparent grade offers high heat deflection temperature, excellent toughness and dimensional stability and resistance to mineral acids. Other desirable properties include thermal stability, creep resistance and inherent flame resistance. Veradel® 3300 Prem MR is FDA compliant and is approved for direct food contact. This grade was formerly marketed as Gafone™ PESU. Applications: Food Service Applications; General Purpose Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; General Purpose; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium Rigidity Information provided by Solvay Specialty Polymers. |