MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow Unival™ DMDB-6240 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: Unival™ DMDB-6240 NT 7 is a multi-purpose polymer designed for high speed production of blow molded containers used to package household industrial chemicals, such as laundry detergent, health and medicinal aids as well as agricultural and food products. The product is specifically designed to provide excellent processing in all extrusion blow molding equipment.
Main Characteristics:
  • Excellent processability
  • High melt strength
  • Excellent ESCR
Compiles with: US FDA 21 CFR 177.1520©3.2a; Canadian HPFB no objection (with limitations)

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520(c)3.2a; Canadian HPFB no objection

Form: Pellets

Processing Method: Blow Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D792
ESCR 100% Igepal® 400 hour
@Temperature 50.0 °C
400 hour
@Temperature 122 °F
F50; ASTM D1693
Melt Flow  0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 43 g/10 min
@Load 21.6 kg,
Temperature 190 °C
43 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM D2240
Tensile Strength at Break 16.5 MPa2400 psiASTM D638
Tensile Strength, Yield 23.8 MPa3450 psiASTM D638
Elongation at Break 770 %770 %ASTM D638
Elongation at Yield 11 %11 %ASTM D638
Flexural Modulus 0.814 GPa118 ksi2% Secant; ASTM D790B
 1.02 GPa148 ksi1% Secant; ASTM D790B
 1.15 GPa167 ksiTangent; ASTM D790B
Tensile Impact Strength 151 kJ/m²72.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °F
Crystallization Temperature 108 °C226 °F
Deflection Temperature at 0.46 MPa (66 psi) 62.8 °C145 °FUnannealed; ASTM D648
Vicat Softening Point 121 °C250 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF572 / 311265

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.