MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemours Teflon™ FEPD 121 Aqueous Fluorinated Ethylene Propylene Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Fluorinated Ethylene Propylene (FEP)

Material Notes: Teflon™ FEPD 121 is an off-white aqueous fluorinated ethylene propylene (FEP) dispersion stabilized with a non-ionic surfactant. It is a general-purpose dispersion that can be used to impart some the unique properties of FEP to end products that would be difficult to make using traditional melt extrusion processes. It can be used to coat or impregnate porous structures, or to make thin films. It can be coated and melt bonded to polytetrafluoroethylene (PTFE) resin or used as a hot melt adhesive. The FEP resin in Teflon™ FEPD 121 is a melt flowable thermoplastic, providing superior properties typical of fluoroplastic resins. Applications: Heat-sealable top coatings for PTFE-coated fabrics for belting, circuit boards, architectural fabrics, and electrical insulation. Cast film for capacitor dielectrics or chemical barriers. Hot melt adhesive for PTFE, PFA, and FEP parts. Metal coatings. Properly processed products (sintered at high temperatures common to the industry) made from Teflon™ FEPD 121 resin can qualify for use in contact with food in compliance with FDA 21 CFR 177.1550 and European Regulation (EU) No. 10/2011.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 55 %% FEP by weight; ASTM D4441-04
pH 10Dispersion; ASTM E70
Brookfield Viscosity 25 cPASTM D2196
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Surfactant Content on PTFE Solids (%)5.5ASTM D4441-04

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8842 / 268769

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.