MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC GELOY™ CR8510 ASA (Europe)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: ASA, excellent weatherability, injection molding.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Water Absorption 0.50 %0.50 %23°C/sat; ISO 62
Moisture Absorption 0.200 %0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow  6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min; ISO 1133
 6.3 g/10 min
@Load 10.0 kg,
Temperature 220 °C
6.3 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 7.8 g/10 min
@Load 3.80 kg,
Temperature 280 °C
7.8 g/10 min
@Load 8.38 lb,
Temperature 536 °F
ASTM D1238
 10 g/10 min
@Load 5.00 kg,
Temperature 260 °C
10 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm³/10 min; ISO 1133
 11 g/10 min
@Load 5.00 kg,
Temperature 260 °C
11 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9393ASTM D785
Tensile Strength at Break 19.0 MPa2760 psi50 mm/min; ISO 527
 33.0 MPa4790 psi50 mm/min; ASTM D638
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min; ASTM D638
 43.0 MPa6240 psi50 mm/min; ISO 527
Elongation at Break 35 %35 %50 mm/min; ISO 527
 60 %60 %50 mm/min; ASTM D638
Elongation at Yield 3.3 %3.3 %50 mm/min; ISO 527
 3.6 %3.6 %50 mm/min; ASTM D638
Tensile Modulus 1.97 GPa286 ksi5 mm/min; ASTM D638
 2.04 GPa296 ksi1mm/min; ISO 527
 2.07 GPa300 ksi50 mm/min; ASTM D638
Flexural Yield Strength 64.0 MPa9280 psi2 mm/min; ISO 178
 68.0 MPa9860 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.06 GPa299 ksi2 mm/min; ISO 178
 2.17 GPa315 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 4.00 J/cm7.49 ft-lb/inASTM D256
 0.600 J/cm
@Temperature -30.0 °C
1.12 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.40 J/cm²6.66 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 30.0 J22.1 ft-lbASTM D3763
 4.00 J
@Temperature -30.0 °C
2.95 ft-lb
@Temperature -22.0 °F
ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dissipation Factor  0.018
@Frequency 100000 Hz
0.018
@Frequency 100000 Hz
ASTM D150
 0.026
@Frequency 1e+6 Hz
0.026
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
46.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
52.8 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Hot Ball Pressure Test 98.0 °C208 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 103 °C217 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 103 °C
@Thickness 3.20 mm
217 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 89.0 °C192 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C
@Thickness 3.20 mm
194 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 98.0 °C208 °FRate B/50; ASTM D1525
 102 °C216 °FRate B/50; ISO 306
 105 °C221 °FRate B/120; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
 
Optical PropertiesMetricEnglishComments
Gloss 94 %94 %60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 220 - 255 °C428 - 491 °FInjection Molding
Zone 1 215 - 250 °C419 - 482 °F
Zone 2 220 - 255 °C428 - 491 °F
Zone 3 230 - 260 °C446 - 500 °F
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 60.0 - 85.0 °C140 - 185 °F
Drying Temperature 85.0 - 90.0 °C185 - 194 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %0.040 %
Back Pressure 0.300 - 1.00 MPa43.5 - 145 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 30 - 80 rpm30 - 80 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10130 / 243597

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.