MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Synthos CM674 Chlorinated Polyethylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chlorinated polyethylene is a heat, weathering and oil resistant elastomer that has used in many wire/cable, hose, automotive and industrial parts for many years.

Characteristics: Lowest chlorine, medium viscosity, semi-crystallinity and good compatibility with PE and PP.

Application: Blended with PE, PP for thermoplastic application

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.20 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength 13.0 MPa
Elongation at Break 700 %
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 50.0 J/g
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 25 %
 
Descriptive Properties
AppearanceWhite powder
Content10 piece/100gImpurity particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW237 / 320268

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.