Applications: Lanthanum is the second most abundant of the rare earths. Lanthanum-rich Lanthanides have been used extensively for cracking reactions in FCC catalysts, especially to manufacture high-octane gasoline from heavy crude oil. Lanthanum-Rich Rare Earth metals play the important roles in hydrogen storage batteries. It is utilized in green phosphors based on the phosphate (La0.4Ce0.45Tb0.15)PO4; in laser crystals based on the Yttrium-Lanthanum-Fluoride (YLF) composition. Lanthanum Metal is the very important raw materials in producing Hydrogen Storage Alloys for NiMH batteries, and is also used to produce other pure Rare Earth metals and specialty alloys. Small amounts of Lanthanum added to Steel improves its malleability, resistance to impact, and ductility; Small amounts of Lanthanum are present in many pool products to remove the Phosphates that feed algae. Lanthanum Metal can be further processed to various shapes of ingots, pieces, wires, foils, slabs, rods, discs and powder.Information provided by Alfa Chemistry Materials. |
Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |