Eastar™ Renew GN071-30 copolyester is a sustainable, clear copolyester used in a variety of packaging and consumer product applications, including food and beverage packaging, general-purpose packaging, flexible film packaging, and consumer products. It is among the easiest resins to extrude into thin films and rigid, thermoformed containers. Eastar™ Renew GN071-30 copolyester enables fast-moving consumer goods brand owners to reduce their consumption of plastics made from fossil feed stocks, satisfy NGO (nongovernmental organizations) and governmental requirements for sustainability, reduce their carbon footprint, and be fast movers in a growing market for sustainable consumer products. Packaging converters prefer Eastar™ Renew GN071-30 copolyester for its best-in-class processing ease, sustainability without compromise, energy efficiency, thermoformability, and versatility. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC-certified circular content by mass balance allocation. Eastar™ Renew GN071-30 copolyester may be used in various food contact applications under the U.S. Food & Drug Administration (FDA) regulations. This product has been GREENGUARD Indoor Air Quality Certified. The GREENGUARD Indoor Air Quality Certified mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, nonprofit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry-independent, third-party testing program for low emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman copolyesters, visit www.greenguard.org. Choose Eastman Chemical Company under the “Manufacturer” category and click search to display a list of our products. Applications - Extruding
- Graphic arts
- Home, garden & automotive packaging
- Mono-layer film food contact
- Multi-layer film food contact
- Packaging component - food contact
- Packaging component films
- Packaging components non food contact
- Protective film
- Transaction cards
- Wood furniture
Key Attributes- Clear, bright, premium appearance
- Easy to extrude
- Easy to thermoform
- Effective barrier properties
- Great for blown film
- Low greenhouse gas (GHG) emissions
- Lower carbon footprint
- Not a material of concern
- PVC alternative
- Polystyrene (PS) alternative
Information provided by Eastman. |