Stitched with high-temperature fibers. Contains no binders. Not changed by exposure to high temperatures. Dimensions 610 mm x 7.6 m 25 mm thickApplications - High-temperature gaskets
- Furnace linings
- General insulation applications
Information provided by Pyrotek. |