MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound PX92248 Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: LNP THERMOCOMP PX92248 compound is based on Nylon 6 resin containing 30% glass fiber. Added features of this grade include: Improved Impact, UV Stabilized.

Features: High Stiffness,Enhanced Ductility,UV Resistant,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 107 MPa15500 psiASTM D638
 107 MPa15500 psi5 mm/min; ASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
 2.5 %2.5 %5 mm/min; ASTM D638
Tensile Modulus 8.84 GPa1280 ksi50 mm/min; ASTM D638
Flexural Strength 179 MPa26000 psiASTM D790
 179 MPa26000 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.22 GPa1050 ksiASTM D790
 7.22 GPa1050 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 138 J102 ft-lbASTM D256
Izod Impact, Unnotched 8.43 J/cm15.8 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
@Thickness 3.20 mm
383 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 265 - 275 °C509 - 527 °F
Zone 3 275 - 290 °C527 - 554 °F
Melt Temperature 265 - 275 °C509 - 527 °FInjection Molding
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81802 / 289749

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.