MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® X-Protect RX07034 Nylon PA66-X FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Starflam X-Protect RX07034 is a glass fiber reinforced PA66 + PA6 compound. Developed for use in Arc chambers and other injection molding applications, it has low smoke and easy processing.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 170 MPaDAM; ISO 527-2
Elongation at Break 2.3 %DAM; ISO 527-2
Flexural Strength 225 MPaDAM; ISO 178
Flexural Modulus 9500 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 30 - 60 secPLC 2; UL 746
 60 - 120 secUL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 213 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 140 °C
@Thickness 0.800 mm
UL 746
 140 °C
@Thickness 1.60 mm
UL 746
UL RTI, Mechanical with Impact 100 °C
@Thickness 0.800 mm
UL 746
 100 °C
@Thickness 1.60 mm
UL 746
UL RTI, Mechanical without Impact 140 °C
@Thickness 0.800 mm
UL 746
 140 °C
@Thickness 1.60 mm
UL 746
Flammability, UL94 HB
@Thickness 0.800 mm
 HB
@Thickness 1.60 mm
Glow Wire Ignition Temperature 750 °C
@Thickness 1.60 mm
IEC 60695-2-13
Glow Wire Flammability Index 725 °C
@Thickness 1.60 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 280 °CInjection
Middle Barrel Temperature 265 - 280 °CInjection
Front Barrel Temperature 280 °CInjection
Melt Temperature 270 - 280 °CInjection
Mold Temperature 60.0 - 90.0 °CInjection
Drying Temperature 75.0 - 85.0 °CInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
 Release agent
Agency RatingsISO, 1043 PA66+PA6 X GF30
AppearanceNatural Color
FeaturesFlame Retardant
 Good Electrical Properties
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8707 / 293368

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.