Product Description: ENGAGE™ 7387 EL Polyolefin Elastomer is a revolutionary butane copolymer with higher molecular weight, better toughness, and higher melt strength than other commercially available polyolefin elastomers. It is well suited for extruded applications such as Wire & Cable. Main Characteristics: - Pellet form
- High melt strength
- Improved toughness
- Talc dusted (untreated, 1 µm)
Applications: Availability: Asia Pacific; Europe; North America Uses: Blending; Compounding; Medium Voltage Insulation; Wire & Cable Applications Agency Ratings: EU No 10/2011 Form: Pellets Information provided by The Dow Chemical Company |