MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRIN™ EXL8543RCC Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP ELCRIN EXL8543RCC is based on Polycarbonate (PC) siloxane copolymer resin. Added features of this grade include: Medium Flow, Colorable and 40% Post Consumer Recycle (PCR) content. This grade is suitable for applications that require improved aesthetics and wider color space to overcome restricted color space of traditional PCR grades.

Features: Post-Consumer Recycled (PCR) content,Aesthetics and Appearance,Colorable,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.23 g/ccISO 1183
Water Absorption 0.14 %
@Time 86400 sec
ASTM D570
 0.15 %
@Time 86400 sec
ISO 62-1
Moisture Absorption 0.0200 %Injection Molding
Viscosity 16 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0077 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0076 cm/cmSABIC method
Melt Flow 17 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 62.0 MPa50 mm/min; ISO 527
 63.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa50 mm/min; ASTM D638
 58.0 MPa50 mm/min; ISO 527
Elongation at Break 100 %50 mm/min; ASTM D638
 130 %50 mm/min; ASTM D638
 132 %50 mm/min; ISO 527
Elongation at Yield 6.2 %50 mm/min; ISO 527
 6.4 %50 mm/min; ASTM D638
Tensile Modulus 2070 MPa50 mm/min; ASTM D638
 2130 MPa1 mm/min; ISO 527
Flexural Strength 91.0 MPa2 mm/min; ISO 178
 97.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2280 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 770 JASTM D256
 190 J
@Temperature -30.0 °C
ASTM D256
 600 J
@Temperature 0.000 °C
ASTM D256
Izod Impact, Unnotched 2700 J/mASTM D4812
Izod Impact, Notched (ISO) 52.0 kJ/m²80*10*4; ISO 180/1A
 16.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 20.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 237 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 330 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 59.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 18.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 23.0 kJ/m²
@Temperature 0.000 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ASTM E831
 66.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ASTM E831
 72.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 139 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 124 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 126 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 142 °CRate B/50; ASTM D1525
 142 °CRate B/50; ISO 306
 144 °CRate B/120; ISO 306
 144 °CRate B/120; ASTM D1525
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.470 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 310 °C
Zone 2 280 - 305 °C
Zone 3 295 - 315 °C
Melt Temperature 295 - 315 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80611 / 288558

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.