MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
EOS Alumide® Nylon 12, Aluminum Filled
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: This metallic gray, aluminum-filled polyamide 12 powder is characterized by high rigidity, a metallic appearance and a range of useful post processing options. The surfaces of Alumide parts can very easily be finished by grinding, polishing or coating. The chip-breaking effect of the aluminum filling simplifies machining. Another impressive property of Alumide® is its very high temperature resistance, which results in excellent dimensional stability at high temperatures. Parts made from Alumide® can therefore be used in functional applications at high temperatures.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 48.0 MPa
Elongation at Break 4.0 %Z
Tensile Modulus 3.80 GPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 175 °C20°C/min
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
 
Descriptive Properties
ColorMetallic gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEOS910 / 280570

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.