MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
JSC SKI-3S AND SKI-5PM Synthetic rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: SKI-3S and SKI-5PM non-specified synthetic cis-isoprene rubbers are cis-polyisoprene obtained by polymerization of isoprene in solution with the usage of stereo specific catalytic complex. Rubbers are stabilized with mixture of two non-staining antioxidants.

Application: used in rubber goods industry for manufacture of light-colored or colored rubbers for noncritical rubber goods.

Appearance: briquette (bale)

Color: from light-white to light-yellow, pink-grey

Information provided by JSC, Synthez-Kauchuk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.5 %
@Time 3600 sec
ASTM D5668
Mooney Viscosity 50 - 100
@Temperature 100 °C
ML 1+4; ASTM D 1646
Storage Temperature <= 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Content>0.04%antioxidants: Tris (2,4-di-tert-butylphenyl) phosphite
 >0.15%antioxidants: Agidol-1 (???)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSC022 / 317842

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.