MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Entec Estane® MB ABHU1 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: Estane® MB ABHU1 is a Polyester TPU based UV stabilizer masterbatch developed for extrusion and molding applications. Incorporation of 2 to 3% Estane® MB ABHU1 in Estane® TPU grades results in molded and extruded articles with an improved UV resistance. To obtain a good dispersion of the UV stabilizer materbatch in the TPU matrix during extrusion/molding, it is advised as screen pack ( up to 100 mesh) during extrusion and sufficient screw back pressure during molding. Recommended to dry MB before processing till = 0.05% moisture.

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Additive: UV Stabilizer

Uses: Masterbatch

Agency Ratings: EC 1907/2006 (REACH)

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 2781
Maximum Moisture Content 0.0500.050Injection
 0.0500.050Extrusion
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 220 °C338 - 428 °FInjection
 170 - 220 °C338 - 428 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENTB671 / 311364

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.