CYCOLOY CY6110 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an impact modified, high flow injection moldable, non chlorinated/brominated flame retardant grade. It features good hydrostability and has a UL94 V0@1.5mm and 5VB@2.5mm flame rating.Information provided by SABIC |