MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mallard Creek Polymers Ecronova® RA 111 Acrylic Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Ecronova RA 111 is a pure acrylic emulsion that provides minimal whitening and good water resistance, especially in mosaic plaster. Due to its high UV Stability, Ecronova RA 111 is recommended for exterior paints and plasters. This product is APE free.

Markets: Paints and Coatings

Applications: Interior Paints, Exterior Paints, Mosaic Plaster

Related Products: Ecronova RA 127, Ecronova KDA 618 eco, Ecronova KDA 788, Ecronova KDA 790, Ecronova KDA 801

Information provided by Mallard Creek Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 49 - 51 %49 - 51 %
pH 7.0 - 9.07.0 - 9.0
Viscosity 3600 - 8000 cP3600 - 8000 cP
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 15.0 °C59.0 °F
 
Descriptive Properties
Minimum Film Formation Temperature (°C)3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMCP9979 / 250414

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.