Polypropylene homopolymer 30% glass fibers/mineral reinforced, chemically coupled, good mechanical properties. Available: all colors, UV stabilized (L), heat stabilized (H), high heat stabilized (HT), laser printable (LP), detergent stabilized (D).Information provided by Taro Plast S.p.a. |