MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Osterman & Co Osterlene® HD0752 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: A high density polyethylene resin and is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. This resin has been designed to provide excellent processability for molders and to met the rigorous performance characteristics of applications requiring stackability, environmental stress crack resistance and impact strength. Applications for HD0752 include injection molding, for injection molded pails, industrial parts and other shipping containers. This product has excellent impact strength, stress crack resistance and processability. It has a very narrow molecular weight distribution. HD0752 has no slip, antiblock or processing aids.

Availability: North America
Features: Good Processability; High ESCR (Stress Crack Resist.); High Impact Resistance; Narrow molecular Weight Distribution
Uses: Containers; Industrial Applications; Pails
Processing Method: Injection Molding

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D792
ESCR 100% Igepal® 12 hourF50; ASTM D1693
Melt Flow 6.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59ASTM D2240
Tensile Strength at Break 3300 psiASTM D638
Tensile Strength, Yield 3900 psiASTM D638
Elongation at Break 1100 %ASTM D638
Elongation at Yield 7.0 %ASTM D638
2% Secant Modulus 155000 psiFlexural; ASTM D790
Tensile Impact Strength 40.0 ft-lb/in²ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Melting Point 268 °F
Crystallization Temperature 244 °F
Deflection Temperature at 0.46 MPa (66 psi) 163 °FUnannealed; ASTM D648
Vicat Softening Point 262 °FASTM D1525
Brittleness Temperature <= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

POSTER031 / 267613

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.