MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

En-Door Reverse ester Tin Heat Stabilizer ED-1318 PVC Heat Stabilizer
Categories: Other Engineering Material

Material Notes: General Information: ED-1318 has excellent high-temperature color stability, long-term dynamic stability and best cost performance. The product is high efficient and environment-friendly without any heavy metal. It can be used to produce PVC pipe with big caliber owing to the good heat stability. Without fouling, the time of cleaning equipment is shortened. The wide rang of processing is especially suitable for double-screw extrusion.

Application: ED-1318 is used in various kinds of pipes, such as PVC-M highly impact pipes, drinking water or drainage pipes, double-wall corrugated pipes, etc. It is also good for rigid sealed strips.

Information provided by En-Door

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 - 1.09 g/cc0.0387 - 0.0394 lb/inĀ³
Viscosity 12 - 20 cP12 - 20 cP
 
Descriptive Properties
AppearanceLight yellow oil liquid
Color<80Pt-Co #

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENDOOR001 / 316635

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.