MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CABELEC® XS6742A PE, Conductive Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product highlights: CABELEC XS6742A conductive concentrate is an electrically conductive concentrate made from a carefully selected carbon black finely dispersed in polyethylene. Its electrical and mechanical properties are not dependent on atmospheric conditions; however, they depend on the type and level of dilution of the resin used and the processing conditions. Unlike standard conductive compounds, which have very limited dilution potential, CABELEC XS6742A conductive concentrate has the potential to be diluted with a high quantity of natural resin. This allows users of CABELEC XS6742A conductive concentrate to benefit from the versatility of this product and from the enhanced physical properties due to higher levels of dilution resin.

Key applications: CABELEC XS6742A conductive concentrate is suitable for extrusion applications where flexibility in the design of a conductive compound formulation is desired and environments where it is desirable to mitigate the hazard of electrostatic discharge.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Melt Flow 0.70 g/10 min
@Load 190 kg,
Temperature 21.6 °C
ISO 1133
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 220 °CExtrusion
Drying Temperature 90.0 °C
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT069 / 315804

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.