MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL™ Resin NHP5054 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NHP5054 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 at 0.75mm for thin-wall molding capability. NORYL NHP5054 is based on a unique co-polymer technology and exhibits good dimensional stability, high heat resistance, strong electrical performance, and very low specific gravity. It is an excellent candidate for electrical vehicle (EV) battery housings, automotive under-the-hood enclosures and components where thin-wall FR, modulus retention, and high heat resistance are required.

Features: Hydrolytic Stability,Low Creep Sensitivity,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.240 %0.240 %23°C / 50% RH; ISO 62
Viscosity 22 cP
@Load 10.0 kg,
Temperature 280 °C
22 cP
@Load 22.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0027 cm/cm0.0027 in/inSABIC method
Melt Flow 24 g/10 min
@Load 10.0 kg,
Temperature 250 °C
24 g/10 min
@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 215 MPa31200 psiH358/30; ISO 2039-1
Tensile Strength at Break 110 MPa16000 psi5 mm/min; ISO 527
Tensile Strength, Yield 120 MPa17400 psi50 mm/min; ASTM D638
Elongation at Break 2.4 %2.4 %5 mm/min; ISO 527
 2.5 %2.5 %5 mm/min; ASTM D638
Tensile Modulus 7.30 GPa1060 ksi1 mm/min; ISO 527
Flexural Strength 145 MPa21000 psiyield, 2 mm/min; ISO 178
 150 MPa21800 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 6.00 GPa870 ksi2.6 mm/min, 100 mm span; ASTM D790
 6.00 GPa870 ksi2 mm/min; ISO 178
Izod Impact Notched 100 J73.8 ft-lbASTM D256
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 3.60 J/cm²
@Temperature -30.0 °C
17.1 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  21.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 32.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
17.8 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  57.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
31.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 103 µm/m-°C
@Temperature 23.0 - 80.0 °C
57.2 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 122 °C252 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 120 °C
@Thickness 6.40 mm
248 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 128 °C262 °FRate B/50; ISO 306
 130 °C266 °FRate B/120; ISO 306
UL RTI, Electrical 125 °C257 °FUL 746B
UL RTI, Mechanical with Impact 115 °C239 °FUL 746B
UL RTI, Mechanical without Impact 125 °C257 °FUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
UL 94
Glow Wire Ignition Temperature  775 °C
@Thickness 1.00 mm
1430 °F
@Thickness 0.0394 in
IEC 60695-2-13
 800 °C
@Thickness 2.00 mm
1470 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 310 °C536 - 590 °F
Zone 2 260 - 305 °C500 - 581 °F
Zone 3 270 - 310 °C518 - 590 °F
Melt Temperature 280 - 310 °C536 - 590 °FInjection Molding
Mold Temperature 75.0 - 105 °C167 - 221 °F
Drying Temperature 105 - 110 °C221 - 230 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82405 / 290352

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.