LNP STAT-KON REL33 compound is based on Nylon 6/6 resin containing 15% carbon fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive Information provided by SABIC |