MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Syensqo (Solvay Specialty Polymers) Tribocomp® PA612 CF30 TS12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes:

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 220 MPa31900 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 19.0 GPa2760 ksiISO 527-2
Flexural Strength 330 MPa47900 psiISO 178
Flexural Modulus 15.0 GPa2180 ksiISO 178
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 ohm100 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C11.7 µin/in-°FISO 11359-2
Thermal Conductivity 0.550 W/m-K3.82 BTU-in/hr-ft²-°FISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Zone 1 220 - 250 °C428 - 482 °FExtrusion
Zone 2 220 - 260 °C428 - 500 °FExtrusion
Zone 3 225 - 270 °C437 - 518 °FExtrusion
Zone 4 230 - 280 °C446 - 536 °FExtrusion
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4557 / 280357

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.