MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® Michem® 2022 Polyurethane Acrylic Hybrid Dispersion
Categories: Fluid; Polymer

Material Notes: Michem® Dispersion Urethanes are water-based polyurethane dispersions that can enhance toughness, scratch resistance, water resistance and flexibility of coatings. Michem Dispersion Urethanes are useful for industrial wood, concrete, and metal substrates. Usage: A tin-free dispersion that provides very good chemical resistance, fast drying and hardening, and abrasion resistance for wood floor and furniture coatings.

Applications (properties imparted): Building Paints (abrasion resistance, chemical resistance, hardness), OEM Applied Wood Protection (abrasion resistance, chemical resistance, gloss enhancement, scratch resistance, wood grain enhancement).

Handling: Avoid contact with eyes, skin and clothing. Ensure adequate ventilation. Handle in accordance with good industrial hygiene and safety practice.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 33 - 36 %33 - 36 %Non-Volatiles
pH 7.0 - 9.07.0 - 9.0
Brookfield Viscosity 20 - 500 cP20 - 500 cPSpindle #2. 20 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceWhite translucent liquid
Emulsifier ChargeAnionic
Minmum Film Forming Temperature (°C)40
Solids TypePolyurethane Acrylic hybrid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9804 / 287399

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.