MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Amodel® FC-1140 STL PPA, 40% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Amodel® FC-1140 STL is an FDA compliant, 40% glass fiber reinforced resin designed for high strength and stiffness along with improved demolding properties. This combines with excellent thermal properties, low water absorption and good hydrolytic stability to make it particularly suited for components used in food service and consumer applications, such coffee machines and ovens.

The STL series of Amodel® PPA was developed specifically for food and beverage applications that require limited impact of polymers on smell, taste and odor.

- Black: FC-1140 STL BK 946
- Natural: FC-1140 STL NT

Applications: Appliances; Consumer Applications; Filters; Housings; Industrial Applications; Plumbing Parts; Pump Parts; Valves/Valve Parts

Features: Chemical Resistant; Chlorine Resistant; Creep Resistant; Good Dimensional Stability; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption; Lubricated

Injection notes: Mold Temperature:
- Minimum mold temperature for typical article thickness is 150°C (302°F). Higher tool temperature might be required for thin wall sections.
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³Method A; ISO 1183
Linear Mold Shrinkage, Flow  0.0016 cm/cm
@Thickness 1.00 mm
0.0016 in/in
@Thickness 0.0394 in
ASTM D955
 0.0018 cm/cm
@Thickness 1.00 mm
0.0018 in/in
@Thickness 0.0394 in
ASTM D955
 0.0021 cm/cm
@Thickness 2.00 mm
0.0021 in/in
@Thickness 0.0787 in
ASTM D955
 0.0025 cm/cm
@Thickness 2.00 mm
0.0025 in/in
@Thickness 0.0787 in
ASTM D955
Linear Mold Shrinkage, Transverse  0.0048 cm/cm
@Thickness 2.00 mm
0.0048 in/in
@Thickness 0.0787 in
ASTM D955
 0.0050 cm/cm
@Thickness 1.00 mm
0.0050 in/in
@Thickness 0.0394 in
ASTM D955
 0.0054 cm/cm
@Thickness 2.00 mm
0.0054 in/in
@Thickness 0.0787 in
ASTM D955
 0.0057 cm/cm
@Thickness 1.00 mm
0.0057 in/in
@Thickness 0.0394 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 260 MPa37700 psiISO 527-2
Elongation at Break 2.2 %2.2 %ISO 527-2
Tensile Modulus 15.3 GPa2220 ksiISO 527-2
Flexural Strength 360 MPa52200 psiISO 178
Flexural Modulus 14.7 GPa2130 ksiISO 178
Charpy Impact Unnotched 8.10 J/cm²38.5 ft-lb/in²ISO 179
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 297 °C567 °FUnannealed, Flatwise; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 315 - 330 °C599 - 626 °F
Middle Barrel Temperature 320 - 340 °C608 - 644 °F
Front Barrel Temperature 325 - 345 °C617 - 653 °F
Melt Temperature 320 - 345 °C608 - 653 °FInjection
Mold Temperature 150 °C302 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Injection
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4115 / 279915

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.