MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECACOMP PEEK LDS black 1047045 Polyetheretherketone, Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes:
  • developed for the LPKF-LDS® process
  • high adhesive strength
  • very good chemical resistance
  • inherent flame retardant
  • good heat deflection temperature
  • low moisture absorption
Target Industries:
  • electrical engineering
  • mechanical engineering
  • medical technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.67 g/cc
Water Absorption at Saturation <= 0.10 %50 % relative humidity up to saturation; DIN EN ISO 62
Linear Mold Shrinkage, Flow 0.0052 cm/cmDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0056 cm/cmDIN EN ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 102 MPaDIN EN ISO 527-1
Elongation at Break 2.3 %DIN EN ISO 527-1
Modulus of Elasticity 10.7 GPaDIN EN ISO 527-1
Charpy Impact Unnotched 31.0 kJ/m²DIN EN ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.6
@Frequency 1e+9 Hz
Dissipation Factor 0.0020
@Frequency 1e+9 Hz
Comparative Tracking Index 225 VDIN EN 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature 23.0 - 100 °C
DIN EN ISO 11359-1;2
 46.0 µm/m-°C
@Temperature 200 - 260 °C
DIN EN ISO 11359-1;2
 63.0 µm/m-°C
@Temperature 260 - 300 °C
DIN EN ISO 11359-1;2
CTE, linear, Transverse to Flow 26.0 µm/m-°C
@Temperature 23.0 - 100 °C
DIN EN ISO 11359-1;2
 67.0 µm/m-°C
@Temperature 200 - 260 °C
DIN EN ISO 11359-1;2
 88.0 µm/m-°C
@Temperature 260 - 300 °C
DIN EN ISO 11359-1;2
Thermal Conductivity 0.500 W/m-Kthrough-plane; ISO 22007-4:2008
 1.70 W/m-Kin-plane; ISO 22007-4:2008
Melting Point 343 °C
Maximum Service Temperature, Air 260 °Clong term
 300 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO-R 75 Method A
Glass Transition Temp, Tg 143 °C
Flammability, UL94 V-0
@Thickness 0.800 mm
DIN IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Processing Temperature 360 - 410 °C
Mold Temperature 170 - 210 °C
Drying Temperature 150 - 160 °C
Dry Time 2.00 - 4.00 hour
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIO9087 / 319015

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.