MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound MF006SXP Polypropylene, Unspecified (PP, Unspecified) (Americas)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP THERMOCOMP MF006SXP compound is based on Polypropylene (PP) resin containing 30% glass fiber. Added features of this grade include: Heat Stabilized.

Features: High Stiffness,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccASTM D792
 1.13 g/ccISO 1183
Moisture Absorption 0.0200 %23°C/50% RH/24 hrs; ASTM D570
 0.0300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm24hrs; ASTM D955
 0.0050 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0096 cm/cm24hrs; ISO 294
 0.010 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 88.0 MPaASTM D638
 91.0 MPaISO 527
Elongation at Break 3.0 %ASTM D638
 3.2 %ISO 527
Tensile Modulus 7300 MPa50 mm/min; ASTM D638
 7600 MPa1 mm/min; ISO 527
Flexural Strength 139 MPaASTM D790
 159 MPaISO 178
Flexural Modulus 6200 MPaASTM D790
 8700 MPaISO 178
Izod Impact Notched 117 JASTM D256
Izod Impact, Unnotched 704 J/mASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 Jpeak; ASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.00 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=1.00 mm
UL 746A
 60 - 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 26.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 26.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 59.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 59.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 152 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 150 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 215 - 225 °C
Zone 3 240 - 250 °C
Melt Temperature 225 - 250 °CInjection Molding
Mold Temperature 30.0 - 50.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81720 / 289667

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.