LNP STAT-KON KEL22A compound is based on Acetal Homopolymer (POM) resin containing 10% carbon fiber, 10% PTFE. Added features of this grade include: Electrically Conductive, Internally Lubricated, Wear Resistant. Features: Internally Lubricated,Light-weight Structural,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive Information provided by SABIC |