MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccASTM D792
Moisture Absorption 0.700 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cmSABIC Method
Linear Mold Shrinkage, Transverse 0.0060 cm/cmSABIC Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 34.0 MPa5 mm/min; ISO 527
 35.0 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 140 %5 mm/min; ISO 527
 200 %Type I, 10 mm/min; SABIC - Japan Method
Tensile Modulus 1170 MPa50 mm/min; ASTM D638
 1190 MPa1 mm/min; ISO 527
Flexural Strength 52.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1150 MPa2 mm/min; ISO 178
 1170 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 580 J/mASTM D256
Charpy Impact, Notched 69.0 kJ/m²ISO 179/2C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+9 - 3.00e+11 ohm-cmASTM D257
Surface Resistance 9.00e+9 - 4.00e+11 ohmASTM D257
Static Decay 2.0 sec5000V to <50V; FTMS101B
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 140 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 25 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 77 %2.54 mm; ASTM D1003

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI53824 / 153870

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.