MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nouryon Ethoquad 18/25 Quat ethoxylated
Categories: Other Engineering Material

Material Notes: Octadecylmethyl[polyoxyethylene (15)] ammonium chloride.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.04 g/cc
@Temperature 50.0 °C
0.0376 lb/in³
@Temperature 122 °F
 1.058 g/cc
@Temperature 25.0 °C
0.03822 lb/in³
@Temperature 77.0 °F
pH 7.0 - 9.07.0 - 9.0
Viscosity  110 cP
@Temperature 90.0 °C
110 cP
@Temperature 194 °F
 1075 cP
@Temperature 37.0 °C
1075 cP
@Temperature 98.6 °F
 1750 cP
@Temperature 23.0 °C
1750 cP
@Temperature 73.4 °F
Vapor Pressure <= 0.000130 bar
@Temperature 20.0 °C
<= 0.0975 torr
@Temperature 68.0 °F
Surface Tension 50 dynes/cm50 dynes/cm0.1% solution
 
Thermal PropertiesMetricEnglishComments
Flash Point 149 °C300 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 150.00 - 15
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 1.0 %1.0 %
 <= 2.0 %<= 2.0 %
 
Descriptive Properties
AppearanceLiquid/Paste
Content= 2 %Free Amine & Amine Salt
 = 95 %Solid content
 = 95 %Active content
Equivalent mass994 g/eq
HLB28Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY541 / 286064

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.