MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL™ FE1410PW PPE+PS (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Glass Filler

Material Notes: Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has been developed for fluid engineering applications that require improved hydrolytic stability. Noryl FE1410PW resin has been certified for potable water applications up to 85C in Europe and North America in limited colors.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Moisture Absorption at Equilibrium 0.060 %50% RH; ASTM D570
Water Absorption at Saturation 0.20 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 32 g/10 min
@Load 10.0 kg,
Temperature 280 °C
MVR, cm^3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 94.0 MPa5 mm/min; ISO 527
 94.0 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 2.7 %5 mm/min; ISO 527
 2.8 %Type I, 5 mm/min; ASTM D638
Flexural Strength 135 MPa2 mm/min; ISO 178
 135 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4860 MPa1.3 mm/min, 50 mm span; ASTM D790
 4880 MPa2 mm/min; ISO 178
Izod Impact, Notched 35.0 J/mASTM D256
 35.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 230 J/mASTM D4812
 225 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1U
 13.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 14.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 14.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²ISO 179/2C
Tangent Modulus 4770 MPa5 mm/min; ASTM D638
 4930 MPa1 mm/min; ISO 527
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 126 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 127 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 140 °CRate B/120; ISO 306
 146 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 280 - 300 °C
Zone 1 250 - 270 °C
Zone 2 270 - 290 °C
Zone 3 290 - 310 °C
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 120 °C
Drying Temperature 100 - 120 °C
Dry Time 2.00 - 4.00 hour
Moisture Content 0.020 %

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI22753 / 215889

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.