MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ MG37EPX ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L)

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 20.6 g/10 min
@Load 10.0 kg,
Temperature 220 °C
20.6 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 39.0 MPa5660 psi5 mm/min; ISO 527
Tensile Strength, Yield 48.0 MPa6960 psi5 mm/min; ISO 527
Elongation at Break 15.8 %15.8 %5 mm/min; ISO 527
Elongation at Yield 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 2.76 GPa400 ksi1mm/min; ISO 527
Flexural Yield Strength 73.0 MPa10600 psi2 mm/min; ISO 178
Flexural Modulus 2.47 GPa358 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 23.0 kJ/m²10.9 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -40.0 °C
2.86 ft-lb/in²
@Temperature -40.0 °F
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 98.0 °C208 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 255 - 280 °C491 - 536 °FInjection Molding
Zone 1 215 - 230 °C419 - 446 °F
Zone 2 230 - 245 °C446 - 473 °F
Zone 3 250 - 270 °C482 - 518 °F
Melt Temperature 255 - 280 °C491 - 536 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 80.0 - 95.0 °C176 - 203 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.050 %0.050 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 70 %50 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10084 / 243551

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.