MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Veradel® HC A-301 Polyethersulfone (PESU)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Veradel® HC A-301 polyethersulfone (PESU) is a rigid, high-temperature, transparent polymer offered for use in high-performance healthcare applications. The material is inherently flame retardant and highly resistant to a wide range of healthcare cleaning and disinfecting agents. It retains its transparency, mechanical properties and dimensional stability in humid, high-heat environments.

Veradel® HC A-301 offers the highest flow rate of all sulfone polymers, making it particularly suited for injection molding thin-walled parts and complex geometries. It is compatible with sterilization via ethylene oxide, vaporized hydrogen peroxide, gamma radiation and steam.

- Natural: Veradel® HC A-301 NT

Applications: Biopharma Processing; Hospital Goods; Medical Device Housings; Medical Devices; Medical/Healthcare Applications; Transparent or Translucent Parts

Features: Acid Resistant; Base Resistant; Biocompatible; Chemical Resistant; Creep Resistant; Detergent Resistant; Ethylene Oxide Sterilizable; Flame Retardant; Food Contact Acceptable; General Purpose; Good Adhesion; Good Dimensional Stability; Good Electrical Properties; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium Rigidity; Radiation (Gamma) Resistant; Radiotranslucent; Steam Sterilizable

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccASTM D792
Water Absorption 0.50 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cmASTM D955
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 380 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 88.9 MPaASTM D638
Elongation at Yield 6.5 %ASTM D638
Tensile Modulus 2690 MPaASTM D638
Flexural Strength 125 MPaASTM D790
Flexural Modulus 2620 MPaASTM D790
Izod Impact, Notched 53.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.70e+15 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
ASTM D150
 3.51
@Frequency 60 Hz
ASTM D150
 3.54
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mmASTM D149
Dissipation Factor 0.0017
@Frequency 60 Hz
ASTM D150
 0.0022
@Frequency 1000 Hz
ASTM D150
 0.0056
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 52.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 200 °CUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 345 - 385 °CInjection
Mold Temperature 149 °C
Drying Temperature 175 °C
@Time 9000 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorTransparent - Slight Yellow
FormsPellets
ProcessingCompounding; Injection Molding
RoHS ComplianceYes
Screw Compression Ratio2.2:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4612 / 280412

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.