MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Celstran® PP-GF20-02 Black PP, 20% Long Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Product Description: Material code according to ISO 104-1: PP Homopolymer reinforced with 20% long glass fibers. Black. The fibers are chemically coupled to the polypropylene matrix. The pellets are cylindrical and normally as well as the embedded fibers 10mm long. This material imparts excellent impact and modulus properties that exceed that short fiber polypropylene.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber

Use: Automotive Applications

Automotive Specifications: BMW GS 93016 Color: (AS3002 BLK); CHRYSLER MS-DB-400 CPN4731 Color: BLK; FORD WSS-M4D865-B5; FORD WSS-M4D865-B7 p>Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccISO 1183
Maximum Moisture Content 0.20
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 12500 psiISO 527-2/5
Elongation at Break 2.4 %ISO 527-2/5
Tensile Modulus 725000 psiISO 527-1
Flexural Strength 12300 psi
@Temperature 80.0 °C
ISO 178
 19600 psi
@Temperature 22.8 °C
ISO 178
Flexural Modulus 479000 psi
@Temperature 80.0 °C
ISO 178
 711000 psi
@Temperature 22.8 °C
ISO 178
Charpy Impact Unnotched 10.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 21.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 6.70 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 7.10 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 316 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Processing Temperature 446 - 482 °FHot Runner
Feed Temperature 68.0 - 122 °FInjection
Rear Barrel Temperature 392 - 428 °F
Middle Barrel Temperature 410 - 446 °F
Front Barrel Temperature 428 - 482 °F
Nozzle Temperature 428 - 482 °F
Zone 4 428 - 482 °FInjection
Melt Temperature 428 - 437 °F
Mold Temperature 86.0 - 158 °F
Drying Temperature 194 - 212 °F
Dry Time 2.00 hour
Back Pressure <= 435 psi
Screw Speed 25 rpm
@Thickness 76.2 mm
 35 rpm
@Thickness 55.9 mm
 50 rpm
@Thickness 40.6 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6247 / 310940

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.