MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Aronkasei AR-830C SEBS
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics:
  • Excellent rubber elasticity and excellent cold resistance
  • Provides anti-slippery products.
  • Natural colors for coloring similar to that of general-use plastics.
  • Reusable scrap such as runners.
  • Provides products 30% lighter than cross-linked rubber.
  • Excellent molten flow characteristics (moldability).
  • Better hygiene than other series (15th edition of Japanese Pharmacopoeia: complied with Food Sanitation Act No. 201).
  • Excellent heat resistance.
  • Excellent resistance against alkali inorganic chemicals.
  • Products having less odor than cross-linked rubber or olefin elastomers.
  • This is suitable for silicone rubber.
Examples of Use: Teethers, ice trays, food tubes, tubes and sheets for medical use, rubber plugs for containers, ear plugs, food container packing, dust-proof masks, milk bottle nipples, various plugs for medical use, and others.

Information provided by ARONKASEI CO.,LTD Elastomer Dept.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccJIS K 7112
Linear Mold Shrinkage 0.0070 - 0.029 cm/cm0.0070 - 0.029 in/in
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.77 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535JIS K 6253 A
Tensile Strength at Break 5.80 MPa841 psiJIS K 6251
Elongation at Break 900 %900 %JIS K 6251
300% Modulus 1.10 MPa160 psiJIS K 6251
Resilience 5858[%]; JIS K 6255
Tear Strength 12.0 kN/m68.5 pliJIS K 6252
Compression Set  10 %
@Temperature 23.0 °C,
Time 86400 sec
10 %
@Temperature 73.4 °F,
Time 24.0 hour
JIS K 6262
 25 %
@Temperature 70.0 °C,
Time 86400 sec
25 %
@Temperature 158 °F,
Time 24.0 hour
JIS K 6262
 65 %
@Temperature 100 °C,
Time 86400 sec
65 %
@Temperature 212 °F,
Time 24.0 hour
JIS K 6262
 
Thermal PropertiesMetricEnglishComments
Softening Point 69.0 °C156 °F
Brittleness Temperature <= -60.0 °C<= -76.0 °FJIS K 6261
 
Descriptive Properties
ColorSemi-transparent (Natural)
Molding MethodInjection / Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJARON008 / 293920

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.