MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-PTFT Post Treatment Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GOYENCHEM-PTFT is high effective synthetic nanometer construction product. It has excellent flame retardant ability and good water solubility. GYC provides complete solution project to the problem of “durability” and “water-resistant” for flame retardant fiber. GOYENCHEM-PTFT, pioneer permanent flame retardant technique, can be applied into construction decoration, high value flame retardant curtain, interior fabric for auto industry, curtain, special working clothes…etc. It’s suitable for synthetic fiber, polyester, T/C blending, artificial fiber, flame retardant for PU coating fabric…etc. Textiles treated with GOYENCHEMPTFT can have permanent and wash resistant flame retardant ability and can be comprehensive applied.

Advantages:

  • GOYENCHEM-PTFT can provide longterm flame retardant ability to fiber
  • The only one special nanometer technique in Asia that makes fabric become excellent wash resistant construction
  • Excellent hand touch after treated with GOYENCHEMPTFT
  • No volatility. Good compatibility with most macromolecule polymer
  • Enhance additional value for various kinds of fiber
  • GOYENCHEM-PTFT has outstanding thermal stability
  • GOYENCHEM-PTFT is environmental friendly and non halogen product
  • GOYENCHEM-PTFT can be added into dyeing bath in first section or do post-treatment
  • GOYENCHEM-PTFT is special nanometer construction and can be added into all kinds of resins to become nanometer fireproof construction layer
Applications
  • Thermosetting resin:phenolic resin, acrylic, epoxy, unsaturated resin, polyester resin, acrylic resin
  • Coating and various resin application: flame retardant coating, all fireproof related acrylic products such as polyurethane resin(PU), PMMA, Latex resins, adhesives
  • Thermoplastic rubber : TPU, PVC, PP, POLYOLIFIN, PET, NYLON, POM, engineering plastics.
  • Rubber industrial: EPDM, CR, NBR,SBR, (SIR), CSM, NR.IIR, and various fireproof rubber.
  • Elastomer:TPE, TPU, SBS, SEBS, TPR, TPV and various elastomer.
  • Foam polymer: can apply on many foam products, especially on flexible and rigid PU, foam, EVA, EPS foaming.
  • Other application: printed ink, paper making, plywood, pigment, print, back adhesives, fireproof masterbatch, textile and various electronic products.

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 - 1.30 g/cc
Particle Size 5.0 - 10 µm
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 5.0mgKOH/g
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.40
 
Descriptive Properties
AppearanceLiquid
ColorTransparent yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN208 / 266516

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.