MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polymer Resources PRL PC-FR-UV2 Non halogen FR PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Flame retardant, halogen free, high impact resistance, medium flow, medium heat resistance, self extinguishing, UV resistant. RoHS compliant.

Polycarbonate is an amorphous engineering polymer that provides exceptional mechanical, thermal, and optical properties. Polycarbonate is one of the only plastics that combine thermal stability, high upper use temperatures (HDT), impact resistance and toughness as well as clarity. Polycarbonate exhibits impact resistance and toughness at a wide range of temperatures. It has superior thermal stability, which yields a large process window for large and small parts. Its amorphous nature gives polycarbonate excellent dimensional stability and uniform shrinkage.

Information provided by Polymer Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/in
@Thickness 3.17 mm
ASTM D955
Melt Flow 9.0 - 16 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9000 psi
@Thickness 3.17 mm
ASTM D638
Tensile Strength, Yield 10000 psi
@Thickness 3.17 mm
ASTM D638
Flexural Strength 13900 psi
@Thickness 3.17 mm
2.00 inch span; ASTM D790
Flexural Modulus 335000 psi
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 15.0 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
Gardner Impact >= 320 in-lb
@Thickness 3.17 mm
ASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 275 °F
@Thickness 3.17 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 265 °F
@Thickness 3.17 mm
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.52 mm
 V-0
@Thickness 3.05 mm
 5VA
@Thickness 3.05 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 550 - 600 °F
Rear Barrel Temperature 520 - 560 °F
Middle Barrel Temperature 540 - 580 °F
Front Barrel Temperature 560 - 600 °F
Mold Temperature 160 - 200 °F
Drying Temperature 245 - 255 °F
Dry Time 3.00 - 4.00 hourRecommended
 <= 8.00 hourMaximum
 
Descriptive Properties
FormPellets
Processing MethodInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYQ284 / 277906

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.