MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Arya Sasol HBM 4265 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HBM4265 is a high molecular weight, high-density polyethylene with broad molecular weight distribution specially developed for producing intermediate bulk containers (IBC) for the packaging of dangerous goods, large blow molding parts and jerry cans. This grade, which is produced by 1-hexene co-monomer, offers very good creep strength, chemical resistance and environmental stress cracking resistance (ESCR), good processability and stiffness. HBM4265 has been produced under Basell license.

Application: Multipurpose Blow Molding Process; Intermediate Bulk Container (IBC); Large Agricultural Tank; Small to Large Jerry Cans; Co-Extrusion

Forms: Pellets

Attribute: High Impact Resistance; Easy Processability Very Good ESCR; Very Good Creep Strength; Good Chemical Resistance

Additives: Antioxidant: Yes; Processing Aid: No; Antiblock: No; Slip Agent: No

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density >= 0.500 g/ccISO 60
Density 0.944 g/ccISO 1183
Environmental Stress Crack Resistance 60 hour
@Pressure 3.50 MPa,
Temperature 80.0 °C
FNCT, 2% Arkopal N100; ISO 16770
Melt Flow 6.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 24.0 MPaISO 527-1, -2
Elongation at Yield 10 %ISO 527-1, -2
Modulus of Elasticity 0.800 GPaISO 527-1, -2
Tensile Impact Strength 160 kJ/m²
@Temperature -30.0 °C
Notched, Type 1, Method 1B; ISO 8256/1B
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CISO 75
Vicat Softening Point 128 °C
@Load 1.02 kg
Method A; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 230 °CExtruder temperature profile
Melt Temperature 205 - 235 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARYA015 / 250469

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.