MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Radel® R-7159 Precolored Resins Polyphenylsulfone (PPSU), Unfilled
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Unfilled, high flow for thin-wall injection molding, for aircraft interiors

Radel® R-7159 pre-colored polyphenylsulfone (PPSU) resins have been developed for commercial aircraft interior applications with strict color requirements. The product complies with applicable FAA regulation 14CFR Part 25 Appendix F, offering vertical flammability resistance, very low smoke generation and low heat release values in the Ohio State University (OSU) rate of heat release method. It also generates low flaming-mode toxic gas emissions.

The resin offers good resistance to most fluids found in the aviation industry including cleaning agents and pesticides. This product is available in pigmented grades to match OEM color standards.

Available grades include:

- White: Radel® R-7159 WH 70913
- White: Radel® R-7159 WH 7363
- Blue: Radel® R-7159 BU 7923
- Gray: Radel® R-7159 GY 714

Markets/Uses: Aircraft / Aircraft Interiors / Infill Panels; Aircraft / Aircraft Interiors / Oxygen Boxes; Aircraft / Aircraft Interiors / Passenger Service Units; Aircraft / Aircraft Interiors / Video Shrouds; Aircraft / Aircraft Interiors / Window Reveals and Shades

Applications: Aerospace Applications; Aircraft Applications; Aircraft Interiors

Features: Chemical Resistant; Detergent Resistant; Flame Retardant; Good Processing Stability; Good Toughness; High Flow; Low Smoke Emission; Low Toxicity; Paintable

Molded part surface appearance is subjective and is not guaranteed.

OSU Peak Heat Release Rate - FAR 25, AppF < 55.0 kW/m²; OSU Total Heat Release - FAR 25, AppF < 20.0 kW·min/m²; Smoke Density - FAR 25, AppF < 5.0 Ds; Toxic Gas Emissions - BSS 7239/ATS 1000/ABD 0031 < 60 ppm; Toxic Gas Emissions - BSS 7239/ATS 1000/ABD 0031 < 1 ppm; Toxic Gas Emissions - BSS 7239/ATS 1000/ABD 0031 < 1 ppm; Toxic Gas Emissions - BSS 7239/ATS 1000/ABD 0031 < 1 ppm; Toxic Gas Emissions - BSS 7239/ATS 1000/ABD 0031 < 5 ppm; Toxic Gas Emissions - BSS 7239/ATS 1000/ABD 0031 < 30 ppm; Vertical Burn - 60 second - FAR 25.853 No Drip; Vertical Burn - 60 second - FAR 25.853 0.0 sec; Vertical Burn - 60 second - FAR 25.853 < 76.2 mm

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccASTM D792
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 380 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 68.9 MPaASTM D638
Elongation at Break >= 10 %51 mm/min; ASTM D638
Tensile Modulus >= 2410 MPaASTM D638
Flexural Strength >= 103 MPaASTM D790
Flexural Modulus >= 2410 MPaASTM D790
Izod Impact, Notched >= 210 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 200 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 354 - 371 °C
Middle Barrel Temperature 360 - 377 °C
Front Barrel Temperature 366 - 382 °C
Nozzle Temperature 360 - 377 °C
Melt Temperature 366 - 388 °CInjection
Mold Temperature 107 - 163 °C
Drying Temperature 149 - 177 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlue; Grey; White
FormsPellets
Injection RateFast
ProcessingInjection Molding
RoHS ComplianceYes
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4400 / 280200

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.